<div dir="ltr">[+3]. On a related note, I had to replace some 82% cotton Velvet with 100% cotton Velvet ONCE to get the 'nap' and 'drape' right. And NO, it was never turned upside down, which was my first guess. It cost me a few bucks.<div>/s/ Richard</div></div><div class="gmail_extra"><br><div class="gmail_quote">On Mon, Feb 1, 2016 at 2:33 PM, Steven Hood via Stagecraft <span dir="ltr"><<a href="mailto:stagecraft@theatrical.net" target="_blank">stagecraft@theatrical.net</a>></span> wrote:<br><blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">We had that problem once. We went back and looked carefully at the fiber content, and it turned out we were getting cotton/poly blend.<br>
<br>
Steven R Hood<br>
<a href="tel:310.756.3555" value="+13107563555" target="_blank">310.756.3555</a><div class="HOEnZb"><div class="h5"><br>
<br>
<br>
<br>
On February 1, 2016 2:28:06 PM Rob Graham via Stagecraft <<a href="mailto:stagecraft@theatrical.net" target="_blank">stagecraft@theatrical.net</a>> wrote:<br>
<br>
<blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">
Greetings Stagecraft Collective:<br>
<br>
We're having an interesting phenomenon happen with some muslin soft<br>
cover flats we're building.<br>
<br>
Admittedly - we're not buying muslin from Rose Brand, but off of<br>
another website, and its probably trying to save a few bucks that has<br>
in the end, undone us.<br>
<br>
Our flats are built using textbook correct application for every step,<br>
and we're prepping them exactly the way both I, and the scene designer<br>
have done multiple times through our respective careers.  The oddity<br>
is that after stretching and applying a glue & water size, our fabric<br>
is relaxing, rather than shrinking.  Neither of us has experienced<br>
this before - and I've built flats using fabric from this supplier<br>
(<a href="http://fabricdirect.com" rel="noreferrer" target="_blank">fabricdirect.com</a>)  in the past without problem - albeit in a<br>
different geographic region.  Our glue densities have been between 2:1<br>
and 4:1 water-to-glue, and the same has happened when using a more<br>
traditional starch-based sizing medium as well.<br>
<br>
Have any of you members of the collective mind experiences similar to<br>
this in your adventures, and what did you do to solve it, if you did.<br>
And yes, we both feel a bit.....silly....over this issue.  Its<br>
happened with flats and drops we've sized over the last few years.<br>
<br>
Thanks,<br>
<br>
Rob Graham<br>
<a href="mailto:photonguide@gmail.com" target="_blank">photonguide@gmail.com</a><br>
<br>
____________________________________________________________<br>
For list information see <<a href="http://stagecraft.theprices.net/" rel="noreferrer" target="_blank">http://stagecraft.theprices.net/</a>><br>
Stagecraft mailing list<br>
<a href="mailto:Stagecraft@theatrical.net" target="_blank">Stagecraft@theatrical.net</a><br>
<a href="http://theatrical.net/mailman/listinfo/stagecraft_theatrical.net" rel="noreferrer" target="_blank">http://theatrical.net/mailman/listinfo/stagecraft_theatrical.net</a><br>
</blockquote>
<br>
<br>
<br>
____________________________________________________________<br>
For list information see <<a href="http://stagecraft.theprices.net/" rel="noreferrer" target="_blank">http://stagecraft.theprices.net/</a>><br>
Stagecraft mailing list<br>
<a href="mailto:Stagecraft@theatrical.net" target="_blank">Stagecraft@theatrical.net</a><br>
<a href="http://theatrical.net/mailman/listinfo/stagecraft_theatrical.net" rel="noreferrer" target="_blank">http://theatrical.net/mailman/listinfo/stagecraft_theatrical.net</a><br>
</div></div></blockquote></div><br><br clear="all"><div><br></div>-- <br><div class="gmail_signature">/s/ Richard<br>_________</div>
</div>